ASTM F2102-2017外科植入物用超高分子量聚乙烯加工樣式氧化程度的評定指南Standard Guide for Evaluating the Extent of Oxidation in Polyethylene Fabricated Forms Intended for Surgical Implants ASTM F2102-2017外科植入物用超高分子量聚乙烯加工樣式氧化程度的評定指南Standard Guide for Evaluating the Extent of Oxidation in Polyethylene Fabricated Forms Intended for Surgical Implants

ASTM F2102-2017外科植入物用超高分子量聚乙烯加工樣式氧化程度的評定指南Standard Guide for Evaluating the Extent of Oxidation in Polyethylene Fabricated Forms Intended for Surgical Implants

  • 標準類(lèi)別:
  • 標準大?。?/li>
  • 標準編號:ASTM F2102-2017
  • 標準狀態(tài):現行
  • 更新時(shí)間:2023-04-23
  • 下載次數:次
標準簡(jiǎn)介

1.1 This guide covers a method for the measurement of the relative extent of oxidation present in HDPE homopolymers and ultra-high-molecular-weight polyethylene (UHMWPE) intended for use in medical implants. The material is analyzed by infrared spectroscopy. The intensity (area) of the carbonyl absorptions (>C=O) centered near 1720 cm-1 is related to the amount of chemically bound oxygen present in the material. Other forms of chemically bound oxygen (C-O-C, C-O-O-C, C-O-H, and so forth) are not captured by this guide. 1.2 Although this guide may give the investigator a means to compare the relative extent of carbonyl oxidation present in various UHMWPE samples, it is recognized that other forms of chemically bound oxygen may be important contributors to these materials' characteristics. 1.3 The applicability of the infrared method has been demonstrated by many literature reports. This particular method, using the intensity (area) of the C-H absorption centered near 1370 cm-1 to normalize for the sample’s thickness, has been validated by an Interlaboratory Study (ILS) conducted according to Practice E691. FIG. 1 Typical FTIR Spectra of Oxidized UHMWPE, Showing the Definition of an Area-Based Oxidation Index Based on Normalization Using the 1370-cm-1 Peak FIG. 2 FTIR Spectra Showing the Carbonyl Absorption Bands Note 1: Note that both reagents effectively extracted the lipids (the lipid absorption peak is centered at approximately 1740 cm-1). The tibial insert was fabricated from highly crosslinked and remelted UHMWPE followed by terminal sterilization in EtO gas (Ref. 1). 1.4 The following precautionary caveat pertains only to the test method portion, Section 5, of this specification: This standard may involve hazardous materials, operations, and equipment. This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this s

標準截圖
版權:如無(wú)特殊注明,文章轉載自網(wǎng)絡(luò ),侵權請聯(lián)系cnmhg168#163.com刪除!文件均為網(wǎng)友上傳,僅供研究和學(xué)習使用,務(wù)必24小時(shí)內刪除。
欧美AAAAAA级午夜福利_国产福利写真片视频在线_91香蕉国产观看免费人人_莉莉精品国产免费手机影院